Author Topic: Woodland Scenics Realistic Water over foam base and the outgassing bubbles  (Read 3532 times)

0 Members and 1 Guest are viewing this topic.

wazzou

  • Crew
  • *
  • Posts: 6728
  • #GoCougs
  • Respect: +1656
I think FlexSeal is pretty expensive and a little overkill when Styrene will likely be just fine.
Bryan

Member of NPRHA, Modeling Committee Member
http://www.nprha.org/
Member of MRHA


MK

  • Crew
  • *
  • Posts: 4065
  • Respect: +772
Heavy Duty aluminum foil would be thicker.

Chris333

  • Crew
  • *
  • Posts: 18395
  • Respect: +5665
a 2x4' sheet of 1/8" Masonite costs less than a 8.5x11" sheet of styrene, just sayin'.

wazzou

  • Crew
  • *
  • Posts: 6728
  • #GoCougs
  • Respect: +1656
a 2x4' sheet of 1/8" Masonite costs less than a 8.5x11" sheet of styrene, just sayin'.


How about a For Sale sign?   :D
Bryan

Member of NPRHA, Modeling Committee Member
http://www.nprha.org/
Member of MRHA


Dave V

  • Crew
  • *
  • Posts: 11222
  • Gender: Male
  • Foothills Farm Studios -- Dave's Model Railroading
  • Respect: +9334
All excellent points!

Chris333

  • Crew
  • *
  • Posts: 18395
  • Respect: +5665
But how do the gases affect styrene  :-X  :trollface:

Dave V

  • Crew
  • *
  • Posts: 11222
  • Gender: Male
  • Foothills Farm Studios -- Dave's Model Railroading
  • Respect: +9334
But how do the gases affect styrene  :-X  :trollface:

Dunno!  One hopes it can't penetrate styrene.  But then again hope is not a strategy.

Chris333

  • Crew
  • *
  • Posts: 18395
  • Respect: +5665
Just kidding, but don't use foam.

wazzou

  • Crew
  • *
  • Posts: 6728
  • #GoCougs
  • Respect: +1656
But how do the gases affect styrene  :-X  :trollface:



The lable said 99.9% safe.    ;)
Bryan

Member of NPRHA, Modeling Committee Member
http://www.nprha.org/
Member of MRHA


MK

  • Crew
  • *
  • Posts: 4065
  • Respect: +772
What's the other 0.01%?   :trollface:

dem34

  • Crew
  • *
  • Posts: 1660
  • Gender: Male
  • Only here to learn through Osmosis
  • Respect: +1192
+1
What's the other 0.01%?   :trollface:

Resonance Cascade.

 :trollface:
-Al

LIRR

  • Crew
  • *
  • Posts: 1285
  • Respect: +1804
0
Use a piece of 1/8 plywood over the foam as a riverbed...sand smooth and paint. I’ve had the WS product on plywood in 2 locations for a couple of years without any problems

Dave V

  • Crew
  • *
  • Posts: 11222
  • Gender: Male
  • Foothills Farm Studios -- Dave's Model Railroading
  • Respect: +9334
0
Not sure when I'm going to start benchwork (before August is through though...I want to do the work in the garage and winter will be here in about 7 weeks) but I'm now planning on using some kind of barrier, wither veneer ply, Masonite, or styrene.  As my Virginia-raised wife would say, "ya'll've made a compelling case."

jon612

  • Posts: 18
  • Respect: +5
0
I'm curious if your problem might be related to the adhesive you are using to secure the foam (extruded polystyrene?)

Most adhesives that come in a tube are not ideal for bonding 2 pieces of polystyrene together. If it stays wet in tube, it will stay wet between the foam for a long time, slowly releasing gas. Most of the adhesives in a tube have a shelf life/ expiration date for this reason. It will dry out but never properly cure.

Dave V

  • Crew
  • *
  • Posts: 11222
  • Gender: Male
  • Foothills Farm Studios -- Dave's Model Railroading
  • Respect: +9334
0
I'm curious if your problem might be related to the adhesive you are using to secure the foam (extruded polystyrene?)

Most adhesives that come in a tube are not ideal for bonding 2 pieces of polystyrene together. If it stays wet in tube, it will stay wet between the foam for a long time, slowly releasing gas. Most of the adhesives in a tube have a shelf life/ expiration date for this reason. It will dry out but never properly cure.

This isn't an issue.  I use foam-compatible construction adhesive only.  Plus it happens in areas where I specifically haven't used adhesive either because the water channel is only part way dug into a 2" slab of foam or because I deliberately left an area unglued in anticipation of it serving as a water surface.